Fixing the technology LEF file.
The technology LEF file was not updated when
https://github.com/google/skywater-pdk/pull/155 was merged.
Technology LEF file changes include;
Signed-off-by: Tim 'mithro' Ansell <tansell@google.com>
diff --git a/tech/sky130_fd_sc_ms.tlef b/tech/sky130_fd_sc_ms.tlef
index ad14973..e26877a 100644
--- a/tech/sky130_fd_sc_ms.tlef
+++ b/tech/sky130_fd_sc_ms.tlef
@@ -28,6 +28,10 @@
MANUFACTURINGGRID 0.005 ;
+PROPERTYDEFINITIONS
+ LAYER LEF58_TYPE STRING ;
+END PROPERTYDEFINITIONS
+
# Standard density, single height
SITE unit
SYMMETRY Y ;
@@ -42,6 +46,16 @@
SIZE 0.48 BY 6.66 ;
END unitdbl
+LAYER nwell
+ TYPE MASTERSLICE ;
+ PROPERTY LEF58_TYPE "TYPE NWELL ;" ;
+END nwell
+
+LAYER pwell
+ TYPE MASTERSLICE ;
+ PROPERTY LEF58_TYPE "TYPE PWELL ;" ;
+END pwell
+
LAYER li1
TYPE ROUTING ;
DIRECTION VERTICAL ;
@@ -56,8 +70,8 @@
WIDTH 0 0.17 ;
AREA 0.0561 ; # LI 6
THICKNESS 0.1 ;
- EDGECAPACITANCE 3.26E-6 ;
- CAPACITANCE CPERSQDIST 36.9E-6 ;
+ EDGECAPACITANCE 40.697E-6 ;
+ CAPACITANCE CPERSQDIST 36.9866E-6 ;
RESISTANCE RPERSQ 12.2 ;
ANTENNADIFFSIDEAREARATIO PWL ( ( 0 75 ) ( 0.0125 75 ) ( 0.0225 85.125 ) ( 22.5 10200 ) ) ;
@@ -96,8 +110,8 @@
ANTENNADIFFSIDEAREARATIO PWL ( ( 0 400 ) ( 0.0125 400 ) ( 0.0225 2609 ) ( 22.5 11600 ) ) ;
- EDGECAPACITANCE 1.79E-6 ;
- CAPACITANCE CPERSQDIST 25.8E-6 ;
+ EDGECAPACITANCE 40.567E-6 ;
+ CAPACITANCE CPERSQDIST 25.7784E-6 ;
DCCURRENTDENSITY AVERAGE 2.8 ; # mA/um Iavg_max at Tj = 90oC
ACCURRENTDENSITY RMS 6.1 ; # mA/um Irms_max at Tj = 90oC
@@ -133,8 +147,8 @@
AREA 0.0676 ; # Met2 6
THICKNESS 0.35 ;
- EDGECAPACITANCE 1.22E-6 ;
- CAPACITANCE CPERSQDIST 17.5E-6 ;
+ EDGECAPACITANCE 37.759E-6 ;
+ CAPACITANCE CPERSQDIST 16.9423E-6 ;
RESISTANCE RPERSQ 0.125 ;
DCCURRENTDENSITY AVERAGE 2.8 ; # mA/um Iavg_max at Tj = 90oC
ACCURRENTDENSITY RMS 6.1 ; # mA/um Irms_max at Tj = 90oC
@@ -168,8 +182,8 @@
AREA 0.24 ; # Met3 6
THICKNESS 0.8 ;
- EDGECAPACITANCE 1.86E-6 ;
- CAPACITANCE CPERSQDIST 12.6E-6 ;
+ EDGECAPACITANCE 40.989E-6 ;
+ CAPACITANCE CPERSQDIST 12.3729E-6 ;
RESISTANCE RPERSQ 0.047 ;
DCCURRENTDENSITY AVERAGE 6.8 ; # mA/um Iavg_max at Tj = 90oC
ACCURRENTDENSITY RMS 14.9 ; # mA/um Irms_max at Tj = 90oC
@@ -204,8 +218,8 @@
THICKNESS 0.8 ;
- EDGECAPACITANCE 1.29E-6 ;
- CAPACITANCE CPERSQDIST 8.67E-6 ;
+ EDGECAPACITANCE 36.676E-6 ;
+ CAPACITANCE CPERSQDIST 8.41537E-6 ;
RESISTANCE RPERSQ 0.047 ;
DCCURRENTDENSITY AVERAGE 6.8 ; # mA/um Iavg_max at Tj = 90oC
ACCURRENTDENSITY RMS 14.9 ; # mA/um Irms_max at Tj = 90oC
@@ -240,8 +254,8 @@
THICKNESS 1.2 ;
- EDGECAPACITANCE 4.96E-6 ;
- CAPACITANCE CPERSQDIST 6.48E-6 ;
+ EDGECAPACITANCE 38.851E-6 ;
+ CAPACITANCE CPERSQDIST 6.32063E-6 ;
RESISTANCE RPERSQ 0.0285 ;
DCCURRENTDENSITY AVERAGE 10.17 ; # mA/um Iavg_max at Tj = 90oC